Synthesis of Eu2+ and Dy3+ doped strontium aluminates and their properties
dc.contributor.author | Rozenberga-Voska, Laura | |
dc.contributor.author | Grabis, Janis | |
dc.contributor.author | Zolotarjovs, Aleksejs | |
dc.date.accessioned | 2020-10-01T13:52:22Z | |
dc.date.available | 2020-10-01T13:52:22Z | |
dc.date.issued | 2017 | |
dc.description | Financial support to this project was provided by National Research Programme (IMIS2). | en_US |
dc.description.abstract | Strontium aluminate phosphors were synthesized by the solution combustion method using citric acid, urea or glycine as reducing agent and europium and dysprosium as dopants. The content of both dopants was in the range of 1-2 mol%. Dependence of phase composition, crystallite size and specific surface area on calcinations temperature, used reducing agents and dopants were determined. Luminescent properties of the calcinated at 1300 °C powders contained SrAl2O4 (90 %) and Sr4Al24O25 (10%) phases with crystallite size of 80 nm were determined. | en_US |
dc.description.sponsorship | IMIS2; Institute of Solid State Physics, University of Latvia as the Center of Excellence has received funding from the European Union’s Horizon 2020 Framework Programme H2020-WIDESPREAD-01-2016-2017-TeamingPhase2 under grant agreement No. 739508, project CAMART² | en_US |
dc.identifier.doi | 10.4028/www.scientific.net/KEM.721.311 | |
dc.identifier.issn | 1013-9826 | |
dc.identifier.uri | https://dspace.lu.lv/dspace/handle/7/52589 | |
dc.language.iso | eng | en_US |
dc.publisher | Trans Tech Publications Ltd. | en_US |
dc.relation | info:eu-repo/grantAgreement/EC/H2020/739508/EU/Centre of Advanced Material Research and Technology Transfer/CAMART² | en_US |
dc.relation.ispartofseries | Key Engineering Materials;721 | |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.subject | Research Subject Categories::NATURAL SCIENCES:Physics | en_US |
dc.subject | strontium aluminate phosphors | en_US |
dc.subject | luminescence | en_US |
dc.subject | solution combustion method | en_US |
dc.subject | specific surface area | en_US |
dc.subject | powder XRD | en_US |